The silent crack: stress corrosion cracking in ammonia vessels

Refrigeration Insights series. Season 2: The enemy within, part 5.

Last week we talked about the corrosion that works under the insulation, on the outside of the pipe. Today we cross the metal wall: stress corrosion cracking (SCC) attacks the internal surface of pressure vessels, in the most awkward place possible: the main welds.

The source is a 2012 IIAR technical paper by Rowe Bansch (Refrigeration Valves & Systems), which reviews real cases, metallurgical analyses and remediation methods.

What SCC is

The mechanism requires three factors to coincide: steel under tensile stress (such as the steel surrounding the major welds), ammonia, and oxygen as a contaminant. When all three coincide, cracks can initiate on the internal surface and propagate through the vessel wall until they create weeping leaks.

The paper is honest about the proportions: severe cracking is not common in refrigeration applications. But that low frequency is precisely what makes it dangerous: nobody expects it, and the vessel that develops it gives no warning from the outside.

The factors that promote it

The review of cases gives a clear profile of the vessel at risk:

1) Metals with high yield strength: the harder steels are more susceptible to SCC.

2) Residual stresses: cold rolling and welding leave internal stresses in the metal that promote cracking, even with no external load.

3) Oxygen in the system: the air that contaminates the ammonia is the third ingredient. Without oxygen, the mechanism does not start.

The water paradox

And here comes the twist that readers of this series will appreciate. Among the observations gathered by the ammonia industry that the paper cites, the first one is counterintuitive: the ammonia is required to contain at least 0.2 percent water.

Wasn't water the silent enemy of the evaporator? Yes. And it is also the classic inhibitor of SCC: that small proportion of water protects the internal surface of the steel against cracking. Water in ammonia is a fine balance: too much degrades thermodynamic performance; none at all leaves the steel exposed. Engineering is the art of managing that kind of tension.

The other two recommendations on the list complete the defense: take precautions so that air does not contaminate the ammonia during charging (again air as the villain, as in the installment on purgers), and stress relieve the vessels after fabrication, or at a minimum use hot formed or stress relieved heads.

What to look at in your plant

The risk profile is built from records questions: do your vessels have a post fabrication stress relief certificate? Were there charging operations or maintenance work where air could have entered? Is the water content of the ammonia in the right range, neither too much nor none at all? For vessels with years in service, internal inspection of the welds with non destructive testing is the only way to know what is happening on the other side of the wall; the paper devotes sections to inspection and to repair methods for tanks that have already experienced SCC.

Practical advice

Three desk checks before any field inspection: look in each vessel's records for the stress relief certificate or the hot formed heads specification; ask for the latest ammonia water content analysis; and review the charging procedures to confirm that they exclude the ingress of air. If any of the three answers does not appear on paper, you already have the agenda for the next shutdown.

Next week we move from corrosion to protection: pressure relief valves, from the basics to the standards.

Source: R. Bansch, “Stress Corrosion Cracking in Ammonia Refrigeration”, Technical Paper #1, IIAR Industrial Refrigeration Conference, 2012. Thermomac is a corporate member of IIAR.